Usoro Rosin Resin SOR – SOR 422
Nkọwapụta
Ọkwa | Ọdịdị | Na-adị nro Poin (℃) | Agba (Ga#) | Uru acid (mg KOH/g) | Solubility (Resin:Toluene=1:1) |
SOR138 | Odo granular / flake | 95±2 | ≤3 | ≤25 | doro anya |
SOR145 | Odo granular / flake | 100±2 | ≤3 | ≤25 | doro anya |
SOR146 | Odo granular / flake | 100±2 | ≤3 | ≤30 | doro anya |
SOR422 | Odo granular / flake | 130±2 | ≤5 | ≤30 | |
SOR424 | Odo granular / flake | 120±2 | ≤3 | ≤30 |
Arụmọrụ ngwaahịa
Rosin resin SOR 422gbazere na coal coke, esters na turpentine solvents, enweghị ike soluble n'ime ihe na-egbu mmanya na-aba n'anya, soluble na mmanụ mmanụ, na miscibility mmanụ oriri dị mma.Ngwaahịa a nwere uru nke agba ọkụ, ọ dịghị mfe ịcha edo edo, nkwụsi ike dị mma na nkwụsi ike siri ike.
Ngwa
Rosin resin SOR422a na-eji polyurethane, agba nitrocellulose, agba amino baking, ink plastik, wdg, iji meziwanye ike, nchapụta, na-egbuke egbuke na njupụta nke ihe nkiri agba, na-ekpo ọkụ gbazee nrapado na ihe ịrịba ama okporo ụzọ na-eme ka adhesion ma ọ bụ onye na-ejikọta ọnụ.
Nkwakọ ngwaahịa
25kg mejupụtara akpa akwụkwọ kraft.
Gịnị mere Họrọ Anyị
Na mgbakwunye, ụlọ ọrụ anyị na-etinye aka na nyocha na mmepe.Anyị na-etinye nnukwu ego na mmepe nke ngwaahịa ọhụrụ na mmelite nke ngwaahịa ndị dị ugbu a iji kwado mkpa mgbanwe nke ahịa.Anyị na-agbasi mbọ ike imeziwanye arụmọrụ na ịdị mma nke ngwaahịa anyị ka anyị na-ebelata mmetụta ha na gburugburu ebe obibi.Site na ntinye aka anyị na nyocha na mmepe, anyị na-anọgide na-ebute ụzọ nke ihe ọhụrụ ma nwee ike ịnye ndị ahịa anyị ihe ngwọta kachasị ọhụrụ na nke dị irè.